Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Glasübergangstemperatur | 178 °C Show Supplier Material materials with Glasübergangstemperatur of 178 °C | ||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.45E-4 - 2.35E-4 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.45E-4 - 2.35E-4 1/K | respectively for below and above Tg |
Max. Betriebstemperatur | 300 °C Show Supplier Material materials with Max. Betriebstemperatur of 300 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Surface Planarization, High Temperature Gap fill, Spin-on Carbon, High temperature thermoset, Semiconductor Industry, Aerospace, Automotive, Packaging, Electronic Packaging |