Allgemein
Property | Value | Comment |
---|---|---|
Korngröße | 2 μm Show Supplier Material materials with Korngröße of 2 μm | Maximum, ASTM E112 |
Abmessung
Property | Value |
---|---|
Länge | 12.7 - 103.6 mm Show Supplier Material materials with Länge of 12.7 - 103.6 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | -60.0 °C | 68 J Show Supplier Material materials with Charpy impact energy, V-notch of 68 J | Average |
Charpy-Schlagenergie, transversal | -60.0 °C | 47 J Show Supplier Material materials with Charpy-Schlagenergie, transversal of 47 J | Single value |
Dehnung | 23.0 °C | 20 % Show Supplier Material materials with Dehnung of 20 % | |
Flächenreduzierung | 23.0 °C | 35 % Show Supplier Material materials with Flächenreduzierung of 35 % | |
Härte, HBW | 23.0 °C | 298 - 363 [-] Show Supplier Material materials with Härte, HBW of 298 - 363 [-] | |
Härte, Rockwell C | 23.0 °C | 32 - 40 [-] Show Supplier Material materials with Härte, Rockwell C of 32 - 40 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 120 - 145 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 120 - 145 MPa | |
Zugfestigkeit | 23.0 °C | 1034 MPa Show Supplier Material materials with Zugfestigkeit of 1034 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.4 - 0.6 % Show Supplier Material materials with Aluminium of 0.4 - 0.6 % | ||
Andere | 4.78 - 5.2 % Show Supplier Material materials with Andere of 4.78 - 5.2 % | Cb+Ta | |
Bismut | 5E-5 % Show Supplier Material materials with Bismut of 5E-5 % | ||
Blei | 1E-3 % Show Supplier Material materials with Blei of 1E-3 % | ||
Bor | 6E-3 % Show Supplier Material materials with Bor of 6E-3 % | ||
Chrom | 17 - 21 % Show Supplier Material materials with Chrom of 17 - 21 % | ||
Eisen | Balance | ||
Kalzium | 3E-3 % Show Supplier Material materials with Kalzium of 3E-3 % | ||
Kobalt | 1 % Show Supplier Material materials with Kobalt of 1 % | ||
Kohlenstoff | 0.045 % Show Supplier Material materials with Kohlenstoff of 0.045 % | ||
Kupfer | 0.23 % Show Supplier Material materials with Kupfer of 0.23 % | ||
Magnesium | 6E-3 % Show Supplier Material materials with Magnesium of 6E-3 % | ||
Mangan | 0.35 % Show Supplier Material materials with Mangan of 0.35 % | ||
Molybdän | 2.8 - 3.3 % Show Supplier Material materials with Molybdän of 2.8 - 3.3 % | ||
Nickel | 55 % Show Supplier Material materials with Nickel of 55 % | ||
Phosphor | 0.01 % Show Supplier Material materials with Phosphor of 0.01 % | ||
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % | ||
Selen | 5E-5 % Show Supplier Material materials with Selen of 5E-5 % | ||
Silizium | 0.35 % Show Supplier Material materials with Silizium of 0.35 % | ||
Titan | 0.8 - 1.15 % Show Supplier Material materials with Titan of 0.8 - 1.15 % |
Technological properties
Property | ||
---|---|---|
Application areas | Ideal applicationsfor Alloy 718 are in oil tools, such as gate valves, choke stems, etc., and high strength applicationssuch as fasteners and turbines. |