Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 10 % Show Supplier Material materials with Dehnung of 10 % |
Härte, Brinell | 23.0 °C | 226 [-] Show Supplier Material materials with Härte, Brinell of 226 [-] |
Härte, Rockwell C | 23.0 °C | 21 [-] Show Supplier Material materials with Härte, Rockwell C of 21 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 555 - 655 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 555 - 655 MPa |
Zugfestigkeit | 23.0 °C | 770 - 828 MPa Show Supplier Material materials with Zugfestigkeit of 770 - 828 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 2 - 4 % Show Supplier Material materials with Aluminium of 2 - 4 % |
Blei | 0.3 % Show Supplier Material materials with Blei of 0.3 % |
Chrom | 0.3 % Show Supplier Material materials with Chrom of 0.3 % |
Eisen | 0.5 - 2.5 % Show Supplier Material materials with Eisen of 0.5 - 2.5 % |
Kupfer | Balance |
Mangan | 0.1 - 1 % Show Supplier Material materials with Mangan of 0.1 - 1 % |
Nickel | 13 - 14 % Show Supplier Material materials with Nickel of 13 - 14 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |
Zink | 0.5 % Show Supplier Material materials with Zink of 0.5 % |
Zinn | 0.3 % Show Supplier Material materials with Zinn of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Bolt | |
Corrosion properties | Used where stress corrosion in ammonia / amine & sulphide environments is an issue. |