Mechanisch
Property | Temperature | Value | |
---|---|---|---|
Dehnung | 23.0 °C | 23 % Show Supplier Material materials with Dehnung of 23 % | |
Härte, Brinell | 23.0 °C | 290 [-] Show Supplier Material materials with Härte, Brinell of 290 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 530 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 530 MPa | |
Zugfestigkeit | 23.0 °C | 730 - 930 MPa Show Supplier Material materials with Zugfestigkeit of 730 - 930 MPa | |
Charpy impact energy, V-notch | 100 |
Chemical properties
Property | Value |
---|---|
Chrom | 24 - 26 % Show Supplier Material materials with Chrom of 24 - 26 % |
Eisen | Balance |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Molybdän | 3 - 4.5 % Show Supplier Material materials with Molybdän of 3 - 4.5 % |
Nickel | 6 - 8 % Show Supplier Material materials with Nickel of 6 - 8 % |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.24 - 0.35 % Show Supplier Material materials with Stickstoff of 0.24 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Corrosion properties | F53 has excellent resistance to stress corrosion cracking in chloride bearing environments, excellent resistance to pitting , crevice and general corrosion. | |
Welding | Good |