Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.43 g/cm³ Show Supplier Material materials with Dichte of 8.43 g/cm³ | |
Korngröße | 4 μm Show Supplier Material materials with Korngröße of 4 μm | Maximum, ASTM E112 |
Abmessung
Property | Value |
---|---|
Länge | 12.7 - 76.2 mm Show Supplier Material materials with Länge of 12.7 - 76.2 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 10 % Show Supplier Material materials with Dehnung of 10 % | ASTM E8, For 50.8mm diameter |
Flächenreduzierung | 23.0 °C | 40 % Show Supplier Material materials with Flächenreduzierung of 40 % | ASTM E8, For 50.8mm diameter |
Härte, Rockwell C | 23.0 °C | 51 [-] Show Supplier Material materials with Härte, Rockwell C of 51 [-] | |
Scherfestigkeit | 23.0 °C | 1034 MPa Show Supplier Material materials with Scherfestigkeit of 1034 MPa | For 25.4mm diameter |
Streckgrenze Rp 0,2 | 23.0 °C | 180 - 210 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 180 - 210 MPa | ASTM E8, Depending on the aging, for 50.8mm diameter |
Zugfestigkeit | 23.0 °C | 190 - 220 MPa Show Supplier Material materials with Zugfestigkeit of 190 - 220 MPa | ASTM E8, Depending on the aging, for 50.8mm diameter |
Chemical properties
Property | Value |
---|---|
Bor | 0.15 % Show Supplier Material materials with Bor of 0.15 % |
Chrom | 19 - 21 % Show Supplier Material materials with Chrom of 19 - 21 % |
Eisen | 1 % Show Supplier Material materials with Eisen of 1 % |
Kobalt | Balance |
Kohlenstoff | 0.025 % Show Supplier Material materials with Kohlenstoff of 0.025 % |
Mangan | 0.15 % Show Supplier Material materials with Mangan of 0.15 % |
Molybdän | 9 - 10.5 % Show Supplier Material materials with Molybdän of 9 - 10.5 % |
Nickel | 33 - 37 % Show Supplier Material materials with Nickel of 33 - 37 % |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % |
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % |
Silizium | 0.15 % Show Supplier Material materials with Silizium of 0.15 % |
Titan | 1 % Show Supplier Material materials with Titan of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | NACE material is ideally suited for oil field equipment such as fasteners, springs, non-magnetic electrical components, instrument parts, valve components, high pressure door fittings, actuators, seals, shafts and other components. | |
Corrosion properties | MP35N in its NACE variant offers exceptional stress corrosion cracking (SCC) resistance for harsh environments such as hydrogen sulphide, salt water and other chloride environments, as well as resists attack from mineral acids (nitric, hydrochloric and sulphur). The material has exceptional resistance to crevice and stress corrosion cracking in sea water and other hostile environments. | |
Processing methods | Melting: MP35N™ is produced by vacuum induction melting followed by VAC-ARC remelting to provide exceptional control of chemistry and ingot solidification. |