Allgemein
Property | Value | Comment |
---|---|---|
Korngröße | 5 μm Show Supplier Material materials with Korngröße of 5 μm | Maximum, ASTM E112 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | 23.0 °C | 27 - 40 J Show Supplier Material materials with Charpy impact energy, V-notch of 27 - 40 J | Depending on the Thickness |
Dehnung | 23.0 °C | 15 % Show Supplier Material materials with Dehnung of 15 % | |
Flächenreduzierung | 23.0 °C | 50 % Show Supplier Material materials with Flächenreduzierung of 50 % | |
Izod Aufprallenergie | 23.0 °C | 27 J Show Supplier Material materials with Izod Aufprallenergie of 27 J | |
Kriechfestigkeit | 450.0 °C | 520 MPa Show Supplier Material materials with Kriechfestigkeit of 520 MPa | For 10000 hours |
500.0 °C | 384 MPa Show Supplier Material materials with Kriechfestigkeit of 384 MPa | For 10000 hours | |
550.0 °C | 261 MPa Show Supplier Material materials with Kriechfestigkeit of 261 MPa | For 10000 hours | |
600.0 °C | 127 MPa Show Supplier Material materials with Kriechfestigkeit of 127 MPa | For 10000 hours | |
Streckgrenze Rp 0,2 | 24.0 °C | 660 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 660 MPa | |
100.0 °C | 624 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 624 MPa | ||
150.0 °C | 603 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 603 MPa | ||
200.0 °C | 595 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 595 MPa | ||
250.0 °C | 581 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 581 MPa | ||
300.0 °C | 573 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 573 MPa | ||
350.0 °C | 559 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 559 MPa | ||
400.0 °C | 537 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 537 MPa | ||
450.0 °C | 508 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 508 MPa | ||
500.0 °C | 464 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 464 MPa | ||
600.0 °C | 406 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 406 MPa | ||
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.015 - 0.08 % Show Supplier Material materials with Aluminium of 0.015 - 0.08 % | ||
Andere | 0.1 % Show Supplier Material materials with Andere of 0.1 % | P+2.43As+3.57Sn+8.16Sb+0.13Cu | |
Arsen | 0.02 % Show Supplier Material materials with Arsen of 0.02 % | ||
Bor | 0.001 - 0.01 % Show Supplier Material materials with Bor of 0.001 - 0.01 % | ||
Chrom | 0.9 - 1.2 % Show Supplier Material materials with Chrom of 0.9 - 1.2 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.17 - 0.23 % Show Supplier Material materials with Kohlenstoff of 0.17 - 0.23 % | ||
Kupfer | 0.2 % Show Supplier Material materials with Kupfer of 0.2 % | ||
Mangan | 0.35 - 0.75 % Show Supplier Material materials with Mangan of 0.35 - 0.75 % | ||
Molybdän | 0.9 - 1.1 % Show Supplier Material materials with Molybdän of 0.9 - 1.1 % | ||
Nickel | 0.2 % Show Supplier Material materials with Nickel of 0.2 % | ||
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | ||
Schwefel | 0.08 % Show Supplier Material materials with Schwefel of 0.08 % | ||
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % | ||
Titan | 0.07 - 0.15 % Show Supplier Material materials with Titan of 0.07 - 0.15 % | ||
Vanadium | 0.6 - 0.8 % Show Supplier Material materials with Vanadium of 0.6 - 0.8 % | ||
Zinn | 0.02 % Show Supplier Material materials with Zinn of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | Fasteners with specified elevated and/or low temperature properties. |