Abmessung
Property | Value |
---|---|
Länge | 12.7 - 127 mm Show Supplier Material materials with Länge of 12.7 - 127 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 15 % Show Supplier Material materials with Dehnung of 15 % | |
Flächenreduzierung | 23.0 °C | 18 % Show Supplier Material materials with Flächenreduzierung of 18 % | |
Härte, Brinell | 23.0 °C | 248 - 321 [-] Show Supplier Material materials with Härte, Brinell of 248 - 321 [-] | |
Härte, Rockwell C | 23.0 °C | 29 - 35 [-] Show Supplier Material materials with Härte, Rockwell C of 29 - 35 [-] | |
Kriechfestigkeit | 650.0 °C | 385 MPa Show Supplier Material materials with Kriechfestigkeit of 385 MPa | For 100 hours resulting in 5% elongation |
Streckgrenze Rp 0,2 | 23.0 °C | 725 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 725 MPa | |
Zugfestigkeit | 23.0 °C | 895 MPa Show Supplier Material materials with Zugfestigkeit of 895 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 - 0.4 % Show Supplier Material materials with Aluminium of 0.3 - 0.4 % |
Bor | 0.0001 - 0.01 % Show Supplier Material materials with Bor of 0.0001 - 0.01 % |
Chrom | 13.5 - 16 % Show Supplier Material materials with Chrom of 13.5 - 16 % |
Eisen | Balance |
Kohlenstoff | 0.07 - 0.09 % Show Supplier Material materials with Kohlenstoff of 0.07 - 0.09 % |
Mangan | 1.96 - 2.04 % Show Supplier Material materials with Mangan of 1.96 - 2.04 % |
Molybdän | 1 - 1.5 % Show Supplier Material materials with Molybdän of 1 - 1.5 % |
Nickel | 24 - 27 % Show Supplier Material materials with Nickel of 24 - 27 % |
Phosphor | 0.04 - 0.05 % Show Supplier Material materials with Phosphor of 0.04 - 0.05 % |
Schwefel | 0.025 - 0.035 % Show Supplier Material materials with Schwefel of 0.025 - 0.035 % |
Silizium | 0.95 - 1.05 % Show Supplier Material materials with Silizium of 0.95 - 1.05 % |
Titan | 1.9 - 2.35 % Show Supplier Material materials with Titan of 1.9 - 2.35 % |
Vanadium | 0.1 - 0.5 % Show Supplier Material materials with Vanadium of 0.1 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Bolts, fasteners, turbines, critical framesin high stress / heat applications, castings and fasteners. |