Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.87 g/cm³ Show Supplier Material materials with Dichte of 8.87 g/cm³ |
Abmessung
Property | Value |
---|---|
Durchmesser | 10 - 250 mm Show Supplier Material materials with Durchmesser of 10 - 250 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 40 % Show Supplier Material materials with Dehnung of 40 % |
Härte, HBW | 23.0 °C | 325 [-] Show Supplier Material materials with Härte, HBW of 325 [-] |
Härte, Rockwell C | 23.0 °C | 35 [-] Show Supplier Material materials with Härte, Rockwell C of 35 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 283 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 283 MPa |
Zugfestigkeit | 23.0 °C | 690 MPa Show Supplier Material materials with Zugfestigkeit of 690 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 14.5 - 16.5 % Show Supplier Material materials with Chrom of 14.5 - 16.5 % |
Eisen | 4 - 7 % Show Supplier Material materials with Eisen of 4 - 7 % |
Kobalt | 2.5 % Show Supplier Material materials with Kobalt of 2.5 % |
Kohlenstoff | 0.01 % Show Supplier Material materials with Kohlenstoff of 0.01 % |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % |
Molybdän | 15 - 17 % Show Supplier Material materials with Molybdän of 15 - 17 % |
Nickel | Balance |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 0.08 % Show Supplier Material materials with Silizium of 0.08 % |
Vanadium | 0.35 % Show Supplier Material materials with Vanadium of 0.35 % |
Wolfram | 3 - 4 % Show Supplier Material materials with Wolfram of 3 - 4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy C276 can be used in the most severe environments such as chemical and petrochemical processing involving bleach, pollution control, pulp and paper production, industrial and municipal waste treatment, pharmaceutical and food processing equipment, and process plant involved in the recovery of sour natural gas. Alloy C276 is ideal for use in evaporators, heat exchangers, sulphuric acid filters and reactors, and process plant handling acid catalysts. | |
Corrosion properties | C276 is resistant to pitting, stress corrosion cracking, and crevice corrosion in a wide range of chemical environments, particularly in chloride gas, hypochlorite and chlorine dioxide solutions. Meanwhile the chromium content adds resistance to oxidizing media, such as ferric and cupric chlorides. To complete the overall corrosion resisting properties, tungsten is present to provide additional general resistance in a wide range of severe environments. | |
Welding | Welding properties are good, with the low carbon content minimizing carbide / grain boundary precipitation during welding to maintain corrosion resistance in the welded finished condition. |