Abmessung
Property | Value |
---|---|
Durchmesser | 12.7 - 250 mm Show Supplier Material materials with Durchmesser of 12.7 - 250 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 30 % Show Supplier Material materials with Dehnung of 30 % |
Elastizitätsmodul | 23.0 °C | 180 GPa Show Supplier Material materials with Elastizitätsmodul of 180 GPa |
Streckgrenze Rp 0,2 | 23.0 °C | 310 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 310 MPa |
Zugfestigkeit | 23.0 °C | 550 MPa Show Supplier Material materials with Zugfestigkeit of 550 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 % Show Supplier Material materials with Aluminium of 0.5 % |
Eisen | 2.5 % Show Supplier Material materials with Eisen of 2.5 % |
Kohlenstoff | 0.3 % Show Supplier Material materials with Kohlenstoff of 0.3 % |
Kupfer | 28 - 34 % Show Supplier Material materials with Kupfer of 28 - 34 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Nickel | 63 - 70 % Show Supplier Material materials with Nickel of 63 - 70 % |
Schwefel | 0.24 % Show Supplier Material materials with Schwefel of 0.24 % |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Valves, Fasteners and Marine engineering, Chemical and hydrocarbon processing equipment, Pumps, Propeller shafts, Oil and fresh water tanks, Fittings, Heat exchangers |