Mechanisch
Property | Temperature | Value | |
---|---|---|---|
Dehnung | 23.0 °C | 25 % Show Supplier Material materials with Dehnung of 25 % | |
Flächenreduzierung | 23.0 °C | 45 % Show Supplier Material materials with Flächenreduzierung of 45 % | |
Härte, Brinell | 23.0 °C | 270 [-] Show Supplier Material materials with Härte, Brinell of 270 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 485 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 485 MPa | |
Zugfestigkeit | 23.0 °C | 655 - 880 MPa Show Supplier Material materials with Zugfestigkeit of 655 - 880 MPa | |
Charpy impact energy, V-notch | 45;-46,100;25 |
Chemical properties
Property | Value |
---|---|
Chrom | 21 - 23 % Show Supplier Material materials with Chrom of 21 - 23 % |
Eisen | Balance |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Molybdän | 2.5 - 3.5 % Show Supplier Material materials with Molybdän of 2.5 - 3.5 % |
Nickel | 4.5 - 6.5 % Show Supplier Material materials with Nickel of 4.5 - 6.5 % |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.1 - 0.22 % Show Supplier Material materials with Stickstoff of 0.1 - 0.22 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications in the power generation and oil & gas industry include pumps, valves, pipework, flanges, bolting, connectors & manifolds. | |
Corrosion properties | F51 resists chloride environments and sulphide stress corrosion. Corrossion Test to ASTM G48 Method A 25°C for 24 hours |