Allgemein
Property | Value |
---|---|
Relative Dichte | 3.85 [-] Show Supplier Material materials with Relative Dichte of 3.85 [-] |
Mechanisch
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 5.4e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.4e-06 1/K | 20-100°C | |
6.5e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.5e-06 1/K | 20-300°C | ||
7.7e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.7e-06 1/K | 20-600°C | ||
8.5e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.5e-06 1/K | 20-1000°C | ||
Max. Betriebstemperatur | 1700 °C Show Supplier Material materials with Max. Betriebstemperatur of 1700 °C | ||
Wärmeleitfähigkeit | 28 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 28 W/(m·K) | ASTM C408 |
Elektrisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 10 [-] Show Supplier Material materials with Dielektrizitätskonstante of 10 [-] | ASTM D150 | ||
Durchschlagfestigkeit | 10 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 10 kV/mm | ASTM D116 | min. | |
Verlustfaktor | 0.0002 [-] Show Supplier Material materials with Verlustfaktor of 0.0002 [-] | ASTM D150 | ||
spezifischer Widerstand | 200 °C | 1e+13 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1e+13 Ω·m | ASTM D257 | |
400 °C | 1e+10 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1e+10 Ω·m | ASTM D257 | ||
600 °C | 1e+09 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1e+09 Ω·m | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | Protection and Insulating Tubes Protection and insulating tubes made from technical ceramics are the first choice in temperature and measurement control situations, whenever safety and stability aspects are required. Ceramic protection tubes and insulating tubes from CeramTec are used in manufacturing devices for temperature measurement and control. Their resistance against aggressive atmospheres even in the most demanding conditions, where temperatures reach up to 1,700°C make CeramTec products the first choice. The various CeramTec alumina ceramics used, such as Rubalit® C799 or Dimulit® C610, are characterized by their excellent electrical insulation and high mechanical strength. CeramTec also offers a slightly porous material Pormulit® C530. CeramTec protection and insulating tubes are manufactured in accordance to DIN 40680 standards. | |
Chemical composition | Al₂O₃: > 99.7% SiO₂: 0.05% Fe₂O₃: 0.06% MgO: 0.15% CaO: 0.025% | |
Color | Off white. |