Allgemein
Abmessung
Property | Value |
---|---|
Breite | 1520 mm Show Supplier Material materials with Breite of 1520 mm |
Dimensions | Standard stock sizes: 1520mm x 3020mm and 12-40mm in thickness |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 5 - 8 % Show Supplier Material materials with Dehnung A50 of 5 - 8 % | |
Elastizitätsmodul | 23.0 °C | 71 GPa Show Supplier Material materials with Elastizitätsmodul of 71 GPa | |
Härte, HBW | 23.0 °C | 158 - 161 [-] Show Supplier Material materials with Härte, HBW of 158 - 161 [-] | Test method: 2.5/62.5 |
Streckgrenze Rp 0,2 | 23.0 °C | 460 - 470 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 460 - 470 MPa | |
Zugfestigkeit | 23.0 °C | 530 - 540 MPa Show Supplier Material materials with Zugfestigkeit of 530 - 540 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.34E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.34E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 862 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 862 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 130 - 160 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 130 - 160 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.90E+7 - 2.30E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.90E+7 - 2.30E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Heat treatable alloy | |
Processing history | Temper: T651 |