Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.7 g/cm³ Show Supplier Material materials with Dichte of 2.7 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Standard stock sizes: 3000mm and 10-300mm in thickness |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 6 - 8 % Show Supplier Material materials with Dehnung A5 of 6 - 8 % | |
Elastizitätsmodul | 23.0 °C | 70 GPa Show Supplier Material materials with Elastizitätsmodul of 70 GPa | |
Härte, HBW | 23.0 °C | 95 [-] Show Supplier Material materials with Härte, HBW of 95 [-] | Test method: 2.5/62.5 |
Streckgrenze Rp 0,2 | 23.0 °C | 200 - 260 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 200 - 260 MPa | |
Zugfestigkeit | 23.0 °C | 270 - 310 MPa Show Supplier Material materials with Zugfestigkeit of 270 - 310 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.34E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.34E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 896 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 896 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 170 - 220 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 170 - 220 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.40E+7 - 3.20E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 2.40E+7 - 3.20E+7 S/m |
Technological properties
Property | ||
---|---|---|
Processing history | Temper: T6, T651, T6511 |