Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.66 g/cm³ Show Supplier Material materials with Dichte of 2.66 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Standard stock sizes: 1520mm x 3020mm and 4-60mm in thickness |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 14 - 16 % Show Supplier Material materials with Dehnung A50 of 14 - 16 % | |
Elastizitätsmodul | 23.0 °C | 70 GPa Show Supplier Material materials with Elastizitätsmodul of 70 GPa | |
Härte, HBW | 23.0 °C | 73 - 75 [-] Show Supplier Material materials with Härte, HBW of 73 - 75 [-] | Test method: 2.5/62.5 |
Streckgrenze Rp 0,2 | 23.0 °C | 115 - 125 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 115 - 125 MPa | |
Zugfestigkeit | 23.0 °C | 270 - 275 MPa Show Supplier Material materials with Zugfestigkeit of 270 - 275 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.42E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.42E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 900 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 900 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 110 - 140 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 110 - 140 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.60E+7 - 1.90E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.60E+7 - 1.90E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Non heat treatable | |
Processing history | Temper: H111 |