Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.76 g/cm³ Show Supplier Material materials with Dichte of 2.76 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Standard stock sizes: 1520mm x 3020mm and 8-100mm in thickness, 1400mm x 3020mm and 110mm in thickness, 1200mm x 3020mm and 120mm in thickness, 1020mm x 3020mm and 130mm in thickness, 950mm x 3020mm and 140mm in thickness |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 6 - 9 % Show Supplier Material materials with Dehnung A50 of 6 - 9 % | |
Elastizitätsmodul | 23.0 °C | 72 GPa Show Supplier Material materials with Elastizitätsmodul of 72 GPa | |
Härte, HBW | 23.0 °C | 167 - 170 [-] Show Supplier Material materials with Härte, HBW of 167 - 170 [-] | Test method: 2.5/62.5 |
Streckgrenze Rp 0,2 | 23.0 °C | 400 - 495 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 400 - 495 MPa | |
Zugfestigkeit | 23.0 °C | 490 - 555 MPa Show Supplier Material materials with Zugfestigkeit of 490 - 555 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.36E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.36E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 862 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 862 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 120 - 150 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 120 - 150 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.80E+7 - 2.20E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.80E+7 - 2.20E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Heat treatable alloy | |
Processing history | Temper: T651 |