Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.8 g/cm³ Show Supplier Material materials with Dichte of 2.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Standard stock sizes: 1520mm x 3020mm and 12-200mm in thickness |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 2 - 8 % Show Supplier Material materials with Dehnung A50 of 2 - 8 % | |
Elastizitätsmodul | 23.0 °C | 71 GPa Show Supplier Material materials with Elastizitätsmodul of 71 GPa | |
Härte, HBW | 23.0 °C | 104 - 160 [-] Show Supplier Material materials with Härte, HBW of 104 - 160 [-] | Test method: 2.5/62.5 |
Streckgrenze Rp 0,2 | 23.0 °C | 240 - 460 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 240 - 460 MPa | |
Zugfestigkeit | 23.0 °C | 360 - 540 MPa Show Supplier Material materials with Zugfestigkeit of 360 - 540 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.34E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.34E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 862 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 862 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 130 - 160 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 130 - 160 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.90E+7 - 2.30E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.90E+7 - 2.30E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Heat treatable alloy | |
Processing history | Temper: T6, T651, T7351 |