Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.75 g/cm³ Show Supplier Material materials with Dichte of 2.75 g/cm³ |
Oberflächenrauigkeit | 0.4 μm Show Supplier Material materials with Oberflächenrauigkeit of 0.4 μm |
Abmessung
Property | Value |
---|---|
Dimensions | Standard stock sizes: 1520mm x 3020mm and 8-80mm in thickness |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 8 - 13 % Show Supplier Material materials with Dehnung A50 of 8 - 13 % | |
Elastizitätsmodul | 23.0 °C | 71 GPa Show Supplier Material materials with Elastizitätsmodul of 71 GPa | |
Härte, HBW | 23.0 °C | 125 - 130 [-] Show Supplier Material materials with Härte, HBW of 125 - 130 [-] | Test method: 2.5/62.5 |
Streckgrenze Rp 0,2 | 23.0 °C | 330 - 370 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 330 - 370 MPa | |
Zugfestigkeit | 23.0 °C | 390 - 420 MPa Show Supplier Material materials with Zugfestigkeit of 390 - 420 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.36E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.36E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 875 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 875 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 135 - 150 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 135 - 150 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.90E+7 - 2.30E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.90E+7 - 2.30E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Non heat treatable | |
Processing history | Temper: T651 |