Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 3.21 g/cm³ Show Supplier Material materials with Dichte of 3.21 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 610 MPa Show Supplier Material materials with Biegefestigkeit of 610 MPa |
Elastizitätsmodul | 23.0 °C | 330 GPa Show Supplier Material materials with Elastizitätsmodul of 330 GPa |
Härte, Vickers | 23.0 °C | 1417 [-] Show Supplier Material materials with Härte, Vickers of 1417 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 6 - 7 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 6 - 7 MPa·√m |
Poissonzahl | 23.0 °C | 0.25 [-] Show Supplier Material materials with Poissonzahl of 0.25 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3E-6 - 3.2E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3E-6 - 3.2E-6 1/K |
Spezifische Wärmekapazität | 23.0 °C | 660 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 660 J/(kg·K) |
Temperaturschockparameter R2 | 550 W/m Show Supplier Material materials with Temperaturschockparameter R2 of 550 W/m | |
Wärmeleitfähigkeit | 23.0 °C | 15 - 20 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 15 - 20 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Durchschlagfestigkeit | 23.0 °C | 13 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 13 kV/mm |
spezifischer Widerstand | 23.0 °C | 1.00E+16 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+16 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | High precision silicon nitride ceramic balls, roller for bearing, pump valve, Thermocouple Protection Sheaths, Electric heating element, Weld Location Pins | |
Processing methods | Gas Press Sintering, Cold Isostatic Press, Dry Press, Precision Machining Processing |