Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.65 - 2.75 g/cm³ Show Supplier Material materials with Dichte of 2.65 - 2.75 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 23.0 °C | 300 GPa Show Supplier Material materials with Elastizitätsmodul of 300 GPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.69E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.69E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 36.6 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 36.6 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | It is widely used in mechanical seals, seal ring, bearing, pump parts, ballistics, chemical production, energy technology, paper manufacturing and as pipe system components. | |
Processing methods | pressureless sintering, reaction-bonded sintering, recrystallization sintering |