Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 5.74 g/cm³ Show Supplier Material materials with Dichte of 5.74 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 1200 MPa Show Supplier Material materials with Biegefestigkeit of 1200 MPa |
Druckfestigkeit | 23.0 °C | 2100 MPa Show Supplier Material materials with Druckfestigkeit of 2100 MPa |
Elastizitätsmodul | 23.0 °C | 210 GPa Show Supplier Material materials with Elastizitätsmodul of 210 GPa |
Härte, Vickers | 23.0 °C | 1295 [-] Show Supplier Material materials with Härte, Vickers of 1295 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 6 - 7 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 6 - 7 MPa·√m |
Poissonzahl | 23.0 °C | 0.22 - 0.23 [-] Show Supplier Material materials with Poissonzahl of 0.22 - 0.23 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 2.5 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 2.5 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | Ceramic Valve components, Ceramic Pump liners, Ceramic Roller, Ceramic Plugs, Ceramic Sleeves, Ceramic Pistons, Ceramic Nozzle, Ceramic balls, Ceramic Spools, Ceramic Shaft, Ceramic Press tooling | |
Processing methods | Ceramic Injection Molding, Low Pressure Injection Molding, Cold Isostatic Press, Dry Press, Precision Machining Processing |