Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 3.02 g/cm³ Show Supplier Material materials with Dichte of 3.02 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Druckfestigkeit | 23.0 °C | 250 MPa Show Supplier Material materials with Druckfestigkeit of 250 MPa |
Elastizitätsmodul | 23.0 °C | 330 GPa Show Supplier Material materials with Elastizitätsmodul of 330 GPa |
Härte, Vickers | 23.0 °C | 2040 [-] Show Supplier Material materials with Härte, Vickers of 2040 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Wärmeleitfähigkeit | 23.0 °C | 45 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 45 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | It is widely used in mechanical seals, seal ring, bearing, pump parts, ballistics, chemical production, energy technology, paper manufacturing and as pipe system components. | |
Processing methods | pressureless sintering, reaction-bonded sintering, recrystallization sintering |