Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 3.7 g/cm³ Show Supplier Material materials with Dichte of 3.7 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 323.7 MPa Show Supplier Material materials with Biegefestigkeit of 323.7 MPa |
Druckfestigkeit | 23.0 °C | 2068 MPa Show Supplier Material materials with Druckfestigkeit of 2068 MPa |
Elastizitätsmodul | 23.0 °C | 280 - 320 GPa Show Supplier Material materials with Elastizitätsmodul of 280 - 320 GPa |
Härte, Vickers | 23.0 °C | 1377 [-] Show Supplier Material materials with Härte, Vickers of 1377 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 4 - 5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4 - 5 MPa·√m |
Poissonzahl | 23.0 °C | 0.22 - 0.23 [-] Show Supplier Material materials with Poissonzahl of 0.22 - 0.23 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.2E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.2E-6 1/K |
Spezifische Wärmekapazität | 23.0 °C | 780 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 780 J/(kg·K) |
Temperaturschockparameter R2 | 200 W/m Show Supplier Material materials with Temperaturschockparameter R2 of 200 W/m | |
Wärmeleitfähigkeit | 23.0 °C | 23 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 23 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Dielektrizitätskonstante | 23.0 °C | 9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 9 [-] |
Durchschlagfestigkeit | 23.0 °C | 15 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 15 kV/mm |
Verlustfaktor | 23.0 °C | 4E-4 [-] Show Supplier Material materials with Verlustfaktor of 4E-4 [-] |
spezifischer Widerstand | 23.0 °C | 1.00E+16 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+16 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Wear ceramic parts: Ceramic Nozzles, Sprayers Cyclones, Homogenising devices, Ceramic Linings, Milling Systems, Ceramic Thread guides - Precision components: Ceramic Measuring Components, Ceramic Control systems, (Micro) dosing valves, Electronic Components, Mechatronics, Optical applications - Machine-construction: Positioning Guide parts, Coatings, Transport ceramic rollers, Ceramic Dies, Textile machine parts, Furnace parts - Rotating equipment: Ceramic Sliding Bearings, Ceramic Ball bearings, Mechanical seals, Ceramic Plungers, Ceramic Valves / fittings, Dosing components - Cutting & moulding: Ceramic knives, Metal-forming tools, Seaming rolls, Ceramic Punches, Drawing dies | |
Processing methods | Ceramic Injection Molding, Low Pressure Injection Molding, Cold Isostatic Press, Dry Press, Precision Machining Processing |