Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 3.1 g/cm³ Show Supplier Material materials with Dichte of 3.1 g/cm³ |
Mechanisch
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.9E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.9E-6 1/K |
Technological properties
Property | ||
---|---|---|
Application areas | Wear ceramic parts: Ceramic Nozzles, Ceramic, Sprayers Cyclones, Homogenising devices, Ceramic Linings, Milling Systems, Ceramic Thread guides - Precision components: Ceramic Measuring Components, Ceramic Control systems, (Micro) dosing valves, Electronic Components, Mechatronics, Optical applications - Machine-construction: Positioning Guide parts, Coatings, Transport ceramic rollers, Ceramic Dies, Textile machine parts, Furnace parts - Rotating equipment: Ceramic Sliding Bearings, Ceramic Ball bearings, Mechanical seals, Ceramic Plungers, Ceramic Valves / fittings, Dosing components - Cutting & moulding: Ceramic knives, Metal-forming tools, Seaming rolls, Ceramic Punches, Drawing dies | |
Processing methods | Dry Press, Precision Machining Processing |