Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 3.3 g/cm³ Show Supplier Material materials with Dichte of 3.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 325 MPa Show Supplier Material materials with Biegefestigkeit of 325 MPa |
Druckfestigkeit | 23.0 °C | 2500 MPa Show Supplier Material materials with Druckfestigkeit of 2500 MPa |
Elastizitätsmodul | 23.0 °C | 320 GPa Show Supplier Material materials with Elastizitätsmodul of 320 GPa |
Härte, Vickers | 23.0 °C | 1020 [-] Show Supplier Material materials with Härte, Vickers of 1020 [-] |
Poissonzahl | 23.0 °C | 0.24 [-] Show Supplier Material materials with Poissonzahl of 0.24 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.6E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.6E-6 1/K |
Spezifische Wärmekapazität | 23.0 °C | 740 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 740 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 190 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 190 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Dielektrizitätskonstante | 23.0 °C | 8.56 [-] Show Supplier Material materials with Dielektrizitätskonstante of 8.56 [-] |
Durchschlagfestigkeit | 23.0 °C | 15 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 15 kV/mm |
Verlustfaktor | 23.0 °C | 2.8E-4 [-] Show Supplier Material materials with Verlustfaktor of 2.8E-4 [-] |
spezifischer Widerstand | 23.0 °C | 1.00E+16 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+16 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Aluminum Nitride Ceramics is ideal for applications where heat dissipation is required. In addition, since it offers a coefficient of thermal expansion (CTE) near that of silicon, and excellent plasma resistance, it is used for: Semiconductor processing equipment components, Ceramic Heat-sinks for high power system, Crucible for Metal Melting, Ceramic Rod, Ceramic Heater, Ceramic Substrate | |
Processing methods | Ceramic Injection Molding, Low Pressure Injection Molding, Cold Isostatic Press, Dry Press, Tape Casting, Precision Machining Processing |