Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2 g/cm³ Show Supplier Material materials with Dichte of 2 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 30 MPa Show Supplier Material materials with Biegefestigkeit of 30 MPa |
Druckfestigkeit | 23.0 °C | 500 MPa Show Supplier Material materials with Druckfestigkeit of 500 MPa |
Härte, Rockwell A | 23.0 °C | 40 [-] Show Supplier Material materials with Härte, Rockwell A of 40 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Filters for gases and liquids; Capillary Electrophoresis; Filtration for heavy metal ions (Cr, Ni etc) in water; High temperature chemical support for gas absorption; High efficiency flow through catalytic supports; Gas burners; Chromatography; Micro trapping systems and bio-catalytic supports; Vacuum holding plates (vacuum chunk); Nano-membrane supports for sensor applications; Micro-bubble diffusers; Fine or micro channels for electrophoresis; Chemical or bio reactor. | |
Processing methods | Low Pressure Injection Molding, Cold Isostatic Press, Dry Press, Precision Machining Processing |