Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 0.91 g/cm³ Show Supplier Material materials with Dichte of 0.91 g/cm³ | ISO 1183 |
Wasserabsorption | 0.01 % Show Supplier Material materials with Wasserabsorption of 0.01 % | ISO 62 |
Mechanisch
Property | Value | Comment | |
---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | min., ISO 527 | |
Elastizitätsmodul | 1 GPa Show Supplier Material materials with Elastizitätsmodul of 1 GPa | ISO 527 | |
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | ISO 527 | |
Hardness, Ball Indentation | 67 MPa Show Supplier Material materials with Hardness, Ball Indentation of 67 MPa | ISO 2039-1 | |
Härte, Shore D | 70 [-] Show Supplier Material materials with Härte, Shore D of 70 [-] | DIN 53505 | |
Schlagfestigkeit, Charpy gekerbt | 50 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 50 kJ/m² | ISO 179 | |
Streckgrenze | 30 MPa Show Supplier Material materials with Streckgrenze of 30 MPa | ISO 527 | |
Schlagzähigkeit, Charpy ungekerbt | No break, ISO 179 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Max. Betriebstemperatur | 100 °C Show Supplier Material materials with Max. Betriebstemperatur of 100 °C | Longterm | |||
Long | |||||
Short | |||||
Min. Betriebstemperatur | 5 °C Show Supplier Material materials with Min. Betriebstemperatur of 5 °C | Longterm | |||
Vicat-Erweichungstemperatur | 91 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 91 °C | ISO 306, VST B50 | |||
Wärmeformbeständigkeitstemperatur | 96 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 96 °C | 0.45 MPa | |||
Entflammbarkeit | HB UL 94 |
Elektrisch
Property | Value | Comment |
---|---|---|
Dielektrizitätskonstante | 2.3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 2.3 [-] | DIN 53483 |
Verlustfaktor | 0.0002 [-] Show Supplier Material materials with Verlustfaktor of 0.0002 [-] | DIN 53483 |
Volume resistivity | 1e+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+16 Ω·cm | min., VDE 0303 |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS,REACH | |
UV resistance | Partly |