Allgemein
Property | Value | Comment |
---|---|---|
Coefficient of friction | 0.3 [-] Show Supplier Material materials with Coefficient of friction of 0.3 [-] | DIN 53375, C, Against dry running steel |
Dichte | 1.39 g/cm³ Show Supplier Material materials with Dichte of 1.39 g/cm³ | ISO 1183 |
Wasserabsorption | 0.2 % Show Supplier Material materials with Wasserabsorption of 0.2 % | ISO 62 |
Mechanisch
Property | Value | Comment | |
---|---|---|---|
Dehnung | 31 % Show Supplier Material materials with Dehnung of 31 % | ISO 527 | |
Elastizitätsmodul | 3 GPa Show Supplier Material materials with Elastizitätsmodul of 3 GPa | ISO 527 | |
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | ISO 527 | |
Hardness, Ball Indentation | 125 MPa Show Supplier Material materials with Hardness, Ball Indentation of 125 MPa | ISO 2039-1 | |
Härte, Shore D | 83 [-] Show Supplier Material materials with Härte, Shore D of 83 [-] | DIN 53505 | |
Schlagfestigkeit, Charpy gekerbt | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | ISO 179 | |
Streckgrenze | 63 MPa Show Supplier Material materials with Streckgrenze of 63 MPa | ISO 527 | |
Schlagzähigkeit, Charpy ungekerbt | No break, ISO 179 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.00012 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00012 1/K | DIN 53752 | |||
Max. Betriebstemperatur | 100 °C Show Supplier Material materials with Max. Betriebstemperatur of 100 °C | Longterm | |||
Long | |||||
Short | |||||
Vicat-Erweichungstemperatur | 150 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 150 °C | ISO 306, VST B50 | |||
Wärmeformbeständigkeitstemperatur | 95 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 95 °C | 2 MPa | |||
Wärmeleitfähigkeit | 0.31 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.31 W/(m·K) | EN 52612 | |||
Entflammbarkeit | HB UL 94 |
Elektrisch
Property | Value | Comment |
---|---|---|
Dielektrizitätskonstante | 3.8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.8 [-] | DIN 53483 |
Durchschlagfestigkeit | 40 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 40 kV/mm | VDE 0303 |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | IEC 60112 |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | min., VDE 0303 |
Verlustfaktor | 0.005 [-] Show Supplier Material materials with Verlustfaktor of 0.005 [-] | DIN 53483 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | min., VDE 0303 |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical engineering, gear wheels, rollers and snap fits | |