Allgemein
Property | Value | Comment |
---|---|---|
Coefficient of friction | 0.3 [-] Show Supplier Material materials with Coefficient of friction of 0.3 [-] | DIN 53375, C, Against dry running steel |
Dichte | 1.39 g/cm³ Show Supplier Material materials with Dichte of 1.39 g/cm³ | ISO 1183 |
Wasserabsorption | 0.25 % Show Supplier Material materials with Wasserabsorption of 0.25 % | ISO 62 |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 15 % Show Supplier Material materials with Dehnung of 15 % | ISO 527 |
Elastizitätsmodul | 4 GPa Show Supplier Material materials with Elastizitätsmodul of 4 GPa | ISO 527 |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | ISO 527 |
Hardness, Ball Indentation | 170 MPa Show Supplier Material materials with Hardness, Ball Indentation of 170 MPa | ISO 2039-1 |
Hardness, Rockwell R | 96 [-] Show Supplier Material materials with Hardness, Rockwell R of 96 [-] | ISO 2039-1 |
Härte, Shore D | 84 [-] Show Supplier Material materials with Härte, Shore D of 84 [-] | DIN 53505 |
Schlagfestigkeit, Charpy gekerbt | 2 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 2 kJ/m² | ISO 179 |
Schlagzähigkeit, Charpy ungekerbt | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | min., ISO 179 |
Streckgrenze | 90 MPa Show Supplier Material materials with Streckgrenze of 90 MPa | ISO 527 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 8e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8e-05 1/K | DIN 53752 | |||
Max. Betriebstemperatur | 100 °C Show Supplier Material materials with Max. Betriebstemperatur of 100 °C | Longterm | |||
Long | |||||
Short | |||||
Min. Betriebstemperatur | -20 °C Show Supplier Material materials with Min. Betriebstemperatur of -20 °C | Longterm | |||
Wärmeformbeständigkeitstemperatur | 80 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 80 °C | 2 MPa | |||
Wärmeleitfähigkeit | 0.29 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.29 W/(m·K) | DIN 52612 | |||
Entflammbarkeit | HB UL 94 |
Elektrisch
Property | Value | Comment |
---|---|---|
Dielektrizitätskonstante | 3.2 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.2 [-] | DIN 53483 |
Durchschlagfestigkeit | 22 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 22 kV/mm | VDE 0303 |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | IEC 60112 |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | min., VDE 0303 |
Verlustfaktor | 0.014 [-] Show Supplier Material materials with Verlustfaktor of 0.014 [-] | DIN 53483 |
Volume resistivity | 1e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm | min., VDE 0303 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts and rollers | |
Certifications | RoHS,REACH |