Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.03 g/cm³ Show Supplier Material materials with Dichte of 1.03 g/cm³ | ISO 1183 |
Wasserabsorption | 1.1 % Show Supplier Material materials with Wasserabsorption of 1.1 % | ISO 62 |
Mechanisch
Property | Value | Comment | |
---|---|---|---|
Biegefestigkeit | 90 MPa Show Supplier Material materials with Biegefestigkeit of 90 MPa | DIN 53452 | |
Dehnung | 10 % Show Supplier Material materials with Dehnung of 10 % | ISO 527 | |
Hardness, Ball Indentation | 106 MPa Show Supplier Material materials with Hardness, Ball Indentation of 106 MPa | DIN 53452 | |
Härte, Shore D | 78 [-] Show Supplier Material materials with Härte, Shore D of 78 [-] | DIN 53505 | |
Schlagfestigkeit, Charpy gekerbt | 8 - 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8 - 12 kJ/m² | ISO 179 | |
Schlagzähigkeit, Charpy ungekerbt | 110 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 110 kJ/m² | ISO 179 | |
Reißfestigkeit | No break, ISO 527 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 8e-05 - 0.0001 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8e-05 - 0.0001 1/K | DIN 52328 | |||
Max. Betriebstemperatur | 120 °C Show Supplier Material materials with Max. Betriebstemperatur of 120 °C | Longterm | |||
Long | |||||
Short | |||||
Min. Betriebstemperatur | -50 °C Show Supplier Material materials with Min. Betriebstemperatur of -50 °C | Longterm | |||
Vicat-Erweichungstemperatur | 182 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 182 °C | ISO 306, VST B50 | |||
190 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 190 °C | ISO 306, VST B50 | ||||
Wärmeformbeständigkeitstemperatur | 185 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 185 °C | 0.45 MPa | |||
190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | 0.45 MPa | ||||
Wärmeleitfähigkeit | 0.23 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.23 W/(m·K) | DIN 52612 | |||
Entflammbarkeit | HB UL 94 |
Elektrisch
Property | Value | Comment |
---|---|---|
Dielektrizitätskonstante | 3.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.5 [-] | DIN 53483 |
Durchschlagfestigkeit | 30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | DIN53480 |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | DIN 53482 |
Verlustfaktor | 0.038 [-] Show Supplier Material materials with Verlustfaktor of 0.038 [-] | DIN 53483 |
Volume resistivity | 2.7e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2.7e+14 Ω·cm | DIN 53482 |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS,REACH |