Allgemein
Property | Value | Comment |
---|---|---|
Coefficient of friction | 0.12 [-] Show Supplier Material materials with Coefficient of friction of 0.12 [-] | DIN 53375, A, Against dry running steel |
Dichte | 0.93 g/cm³ Show Supplier Material materials with Dichte of 0.93 g/cm³ | ISO 1183 |
Wasserabsorption | 0.01 % Show Supplier Material materials with Wasserabsorption of 0.01 % | ISO 62 |
Mechanisch
Property | Value | Comment | |
---|---|---|---|
Biegefestigkeit | 27 MPa Show Supplier Material materials with Biegefestigkeit of 27 MPa | ISO 178 | |
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | min., ISO 527 | |
Elastizitätsmodul | 0.7 GPa Show Supplier Material materials with Elastizitätsmodul of 0.7 GPa | min., ISO 527 | |
Elongation at yield | 8 % Show Supplier Material materials with Elongation at yield of 8 % | min., ISO 527 | |
Hardness, Ball Indentation | 38 MPa Show Supplier Material materials with Hardness, Ball Indentation of 38 MPa | ISO 2039-1 | |
Härte, Shore D | 63 [-] Show Supplier Material materials with Härte, Shore D of 63 [-] | DIN 53505 | |
Reißfestigkeit | 40 kN/m Show Supplier Material materials with Reißfestigkeit of 40 kN/m | min., ISO 527 | |
Streckgrenze | 17 MPa Show Supplier Material materials with Streckgrenze of 17 MPa | ISO 527 | |
Schlagfestigkeit, Charpy gekerbt | No break, ISO 179 | ||
Schlagzähigkeit, Charpy ungekerbt | No break, ISO 179 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.0002 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.0002 1/K | DIN 53752 | |||
Max. Betriebstemperatur | 90 °C Show Supplier Material materials with Max. Betriebstemperatur of 90 °C | Longterm | |||
Long | |||||
Short | |||||
Min. Betriebstemperatur | -150 °C Show Supplier Material materials with Min. Betriebstemperatur of -150 °C | Longterm | |||
Vicat-Erweichungstemperatur | 79 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 79 °C | ISO 306, VST B50 | |||
Wärmeformbeständigkeitstemperatur | 42 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 42 °C | 2 MPa | |||
65 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 65 °C | 0.45 MPa | ||||
Wärmeleitfähigkeit | 0.41 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.41 W/(m·K) | DIN 52612 | |||
Entflammbarkeit | HB UL 94 |
Elektrisch
Property | Value | Comment |
---|---|---|
Dielektrizitätskonstante | 3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3 [-] | DIN 53483 |
Durchschlagfestigkeit | 45 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 45 kV/mm | VDE 0303 |
Surface resistivity | 1e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+11 Ω/sq | min., VDE 0303 |
Verlustfaktor | 0.0001 [-] Show Supplier Material materials with Verlustfaktor of 0.0001 [-] | DIN 53483 |
Volume resistivity | 1e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm | min., VDE 0303 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, chain guidance and sliding profiles | |
Certifications | Food Contact: FDA and EU 10/2011, RoHS,REACH |