Allgemein
Property | Value | Comment |
---|---|---|
Coefficient of friction | 0.08 [-] Show Supplier Material materials with Coefficient of friction of 0.08 [-] | DIN 53375, A, Against dry running steel |
Dichte | 0.93 g/cm³ Show Supplier Material materials with Dichte of 0.93 g/cm³ | ISO 1183 |
Wasserabsorption | 0.01 % Show Supplier Material materials with Wasserabsorption of 0.01 % | ISO 62 |
Mechanisch
Property | Value | Comment | |
---|---|---|---|
Biegefestigkeit | 27 MPa Show Supplier Material materials with Biegefestigkeit of 27 MPa | ISO 178 | |
Elastizitätsmodul | 0.68 GPa Show Supplier Material materials with Elastizitätsmodul of 0.68 GPa | min., ISO 527 | |
Elongation at yield | 20 % Show Supplier Material materials with Elongation at yield of 20 % | ISO 527 | |
Hardness, Ball Indentation | 35 MPa Show Supplier Material materials with Hardness, Ball Indentation of 35 MPa | ||
Härte, Shore D | 61 [-] Show Supplier Material materials with Härte, Shore D of 61 [-] | DIN 53505 | |
Streckgrenze | 17 MPa Show Supplier Material materials with Streckgrenze of 17 MPa | ISO 527 | |
Zugfestigkeit | 28 MPa Show Supplier Material materials with Zugfestigkeit of 28 MPa | DIN 53455 | |
Dehnung | No break, ISO 527 | ||
Reißfestigkeit | No break, ISO 527 | ||
Schlagfestigkeit, Charpy gekerbt | No break, ISO 179 | ||
Schlagzähigkeit, Charpy ungekerbt | No break, ISO 179 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.0002 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.0002 1/K | DIN 53752 | |||
Max. Betriebstemperatur | 80 °C Show Supplier Material materials with Max. Betriebstemperatur of 80 °C | Longterm | |||
Long | |||||
Short | |||||
Min. Betriebstemperatur | -150 °C Show Supplier Material materials with Min. Betriebstemperatur of -150 °C | Longterm | |||
Vicat-Erweichungstemperatur | 80 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 80 °C | ISO 306, VST B50 | |||
Wärmeformbeständigkeitstemperatur | 42 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 42 °C | 0.45 MPa | |||
Wärmeleitfähigkeit | 0.41 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.41 W/(m·K) | DIN 52612 | |||
Entflammbarkeit | HB UL 94 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, chain guidance and sliding profiles | |
Certifications | Food Contact: FDA and EU 10/2011, RoHS,REACH |