Allgemein
Property | Value | Comment |
---|---|---|
Coefficient of friction | 0.34 [-] Show Supplier Material materials with Coefficient of friction of 0.34 [-] | DIN 53375, C, Against dry running steel |
Dichte | 1.18 g/cm³ Show Supplier Material materials with Dichte of 1.18 g/cm³ | ISO 1183 |
Wasserabsorption | 3.7 % Show Supplier Material materials with Wasserabsorption of 3.7 % | ISO 62 |
Mechanisch
Property | Value | Comment |
---|---|---|
Elastizitätsmodul | 3 GPa Show Supplier Material materials with Elastizitätsmodul of 3 GPa | ISO 527 |
Härte, Shore D | 84 [-] Show Supplier Material materials with Härte, Shore D of 84 [-] | ISO 868 |
Schlagzähigkeit, Charpy ungekerbt | 6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 6 kJ/m² | ISO 179 |
Streckgrenze | 95 MPa Show Supplier Material materials with Streckgrenze of 95 MPa | ISO 527 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Max. Betriebstemperatur | 155 °C Show Supplier Material materials with Max. Betriebstemperatur of 155 °C | Longterm | |
Long | |||
Short | |||
Min. Betriebstemperatur | -40 °C Show Supplier Material materials with Min. Betriebstemperatur of -40 °C | Longterm | |
Wärmeleitfähigkeit | 0.3 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.3 W/(m·K) | DIN 52612 | |
Entflammbarkeit | HB UL 94 |
Elektrisch
Property | Value | Comment |
---|---|---|
Surface resistivity | 1e+16 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+16 Ω/sq | DIN 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, rollers and bushings | |
Certifications | RoHS,REACH |