Allgemein
Property | Value | Comment |
---|---|---|
Coefficient of friction | 0.3 [-] Show Supplier Material materials with Coefficient of friction of 0.3 [-] | DIN 53375, C, Against dry running steel |
Dichte | 1.15 g/cm³ Show Supplier Material materials with Dichte of 1.15 g/cm³ | ISO 1183 |
Wasserabsorption | 2.2 % Show Supplier Material materials with Wasserabsorption of 2.2 % | ISO 62 |
Mechanisch
Property | Value | Comment |
---|---|---|
Elastizitätsmodul | 3 GPa Show Supplier Material materials with Elastizitätsmodul of 3 GPa | ISO 527 |
Härte, Shore D | 83 [-] Show Supplier Material materials with Härte, Shore D of 83 [-] | ISO 868 |
Schlagzähigkeit, Charpy ungekerbt | 3 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 3 kJ/m² | min., ISO 179 |
Streckgrenze | 75 MPa Show Supplier Material materials with Streckgrenze of 75 MPa | ISO 527 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Max. Betriebstemperatur | 100 °C Show Supplier Material materials with Max. Betriebstemperatur of 100 °C | Longterm | |
Long | |||
Short | |||
Min. Betriebstemperatur | -40 °C Show Supplier Material materials with Min. Betriebstemperatur of -40 °C | Longterm | |
Wärmeleitfähigkeit | 0.25 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.25 W/(m·K) | DIN 52612 | |
Entflammbarkeit | V2 UL 94 |
Elektrisch
Property | Value | Comment |
---|---|---|
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | DIN 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, rollers and impact stressed parts | |
Certifications | RoHS,REACH |