Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.48 g/cm³ Show Supplier Material materials with Dichte of 1.48 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 260 MPa Show Supplier Material materials with Biegefestigkeit of 260 MPa | ASTM D790 |
Dehnung | 23.0 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 20 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 20 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 176 MPa Show Supplier Material materials with Zugfestigkeit of 176 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Wärmeformbeständigkeitstemperatur | 210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | ASTM D648 | |
Entflammbarkeit | UL 94 HB (1.6mm) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 17 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 17 kV/mm | ASTM D147 |
Surface resistivity | 23.0 °C | 1.00E+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+12 Ω/sq | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Additives | Halogen-Free Flame Retardant | |
Application areas | Auto parts, power tools, wipers | |
Fillers | 45% Glass Fiber |