Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.3 g/cm³ Show Supplier Material materials with Dichte of 1.3 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 280 MPa Show Supplier Material materials with Biegefestigkeit of 280 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 11.38 GPa Show Supplier Material materials with Biegemodul of 11.38 GPa | ASTM D790 |
Dehnung | 23.0 °C | 2.7 % Show Supplier Material materials with Dehnung of 2.7 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 11.48 GPa Show Supplier Material materials with Elastizitätsmodul of 11.48 GPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 58 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 58 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 220 MPa Show Supplier Material materials with Zugfestigkeit of 220 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Wärmeformbeständigkeitstemperatur | 261 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 261 °C | ASTM D648 | |
Entflammbarkeit | UL 94 V0 |
Technological properties
Property |
---|