Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.51 g/cm³ Show Supplier Material materials with Dichte of 1.51 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 170 MPa Show Supplier Material materials with Biegefestigkeit of 170 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 11.4 GPa Show Supplier Material materials with Biegemodul of 11.4 GPa | ASTM D790 |
Härte, Shore D | 23.0 °C | 84 [-] Show Supplier Material materials with Härte, Shore D of 84 [-] | ASTM D785 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 80 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 80 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 125 MPa Show Supplier Material materials with Zugfestigkeit of 125 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Wärmeformbeständigkeitstemperatur | 264 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 264 °C | ASTM D648 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive bumpers, Automotive applications, Automotive exterior parts | |
Fillers | 20% Glass Fiber |