Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Dichte of 1.27 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 320 MPa Show Supplier Material materials with Biegefestigkeit of 320 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 15.23 GPa Show Supplier Material materials with Biegemodul of 15.23 GPa | ASTM D790 |
Dehnung | 23.0 °C | 2 - 3 % Show Supplier Material materials with Dehnung of 2 - 3 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 106 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 106 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 201 MPa Show Supplier Material materials with Zugfestigkeit of 201 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Wärmeformbeständigkeitstemperatur | 220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | ASTM D648 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+15 Ω/sq | ASTM D257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.1 - 0.2 % Show Supplier Material materials with Schrumpfung of 0.1 - 0.2 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Carbon Fiber |