Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.02 g/cm³ Show Supplier Material materials with Dichte of 1.02 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 60 MPa Show Supplier Material materials with Biegefestigkeit of 60 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 1.8 GPa Show Supplier Material materials with Biegemodul of 1.8 GPa | ASTM D790 |
Dehnung | 23.0 °C | 35 % Show Supplier Material materials with Dehnung of 35 % | Minimum, ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 60 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 60 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 48 MPa Show Supplier Material materials with Zugfestigkeit of 48 MPa | ASTM D638 |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | ASTM D147 |
Surface resistivity | 23.0 °C | 1.00E+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Additives | Toughening Additive | |
Application areas | Wheels, electrical shell, automotive parts, rollers, sports equipment |