Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.42 g/cm³ Show Supplier Material materials with Dichte of 1.42 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 248 MPa Show Supplier Material materials with Biegefestigkeit of 248 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 15.9 GPa Show Supplier Material materials with Biegemodul of 15.9 GPa | ASTM D790 |
Dehnung | 23.0 °C | 1 % Show Supplier Material materials with Dehnung of 1 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 85 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 85 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 214 MPa Show Supplier Material materials with Zugfestigkeit of 214 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 288 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 288 °C | ASTM D648 | |
Entflammbarkeit | UL94 v0 |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 0.1 % Show Supplier Material materials with Schrumpfung of 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Aircraft parts, engine inner covers, bearings, gaskets, seals, clutch gear rings, valves and pumps, semiconductor industry, chemical industry, bars, surgical and dental equipment, military materials | |
Fillers | 30% Carbon Fiber |