Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.33 g/cm³ Show Supplier Material materials with Dichte of 1.33 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 82 MPa Show Supplier Material materials with Biegefestigkeit of 82 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 3 GPa Show Supplier Material materials with Biegemodul of 3 GPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 7.5 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 7.5 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 55 MPa Show Supplier Material materials with Zugfestigkeit of 55 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Wärmeformbeständigkeitstemperatur | 220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | ASTM D648 | |
Entflammbarkeit | UL 94 V0 (1.6mm) |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 1.2 - 1.3 % Show Supplier Material materials with Schrumpfung of 1.2 - 1.3 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Additives | Brominated flame retardant Additive |