Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.42 g/cm³ Show Supplier Material materials with Dichte of 1.42 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 167 MPa Show Supplier Material materials with Biegefestigkeit of 167 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 7.22 GPa Show Supplier Material materials with Biegemodul of 7.22 GPa | ASTM D790 |
Dehnung | 23.0 °C | 6 % Show Supplier Material materials with Dehnung of 6 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 18 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 18 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 136 MPa Show Supplier Material materials with Zugfestigkeit of 136 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.3 - 0.4 % Show Supplier Material materials with Schrumpfung of 0.3 - 0.4 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Additives | Brominated flame retardant | |
Fillers | 25% Glass Fiber |