Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Dichte of 1.27 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 165 MPa Show Supplier Material materials with Biegefestigkeit of 165 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 3.52 GPa Show Supplier Material materials with Biegemodul of 3.52 GPa | ASTM D790 |
Dehnung | 23.0 °C | 60 % Show Supplier Material materials with Dehnung of 60 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 53 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 110 MPa Show Supplier Material materials with Zugfestigkeit of 110 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 201 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 201 °C | ASTM D648 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 33 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 33 kV/mm | ASTM D147 |
Technological properties
Property |
---|