Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.24 g/cm³ Show Supplier Material materials with Dichte of 1.24 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 172 MPa Show Supplier Material materials with Biegefestigkeit of 172 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 2.76 GPa Show Supplier Material materials with Biegemodul of 2.76 GPa | ASTM D790 |
Dehnung | 23.0 °C | 10 % Show Supplier Material materials with Dehnung of 10 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 91 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 91 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 86.2 MPa Show Supplier Material materials with Zugfestigkeit of 86.2 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 133 °C | ASTM D648 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+12 Ω/sq | ASTM D257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.2 - 0.3 % Show Supplier Material materials with Schrumpfung of 0.2 - 0.3 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Additives | Flame Retardant |