Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 93.2 MPa Show Supplier Material materials with Biegefestigkeit of 93.2 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 2.26 GPa Show Supplier Material materials with Biegemodul of 2.26 GPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 12 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 12 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 61.8 MPa Show Supplier Material materials with Zugfestigkeit of 61.8 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 125 °C | ASTM D648 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.6 % Show Supplier Material materials with Schrumpfung of 0.6 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Additives | Light Diffusion |