Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.34 g/cm³ Show Supplier Material materials with Dichte of 1.34 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 62.1 MPa Show Supplier Material materials with Biegefestigkeit of 62.1 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 1.93 GPa Show Supplier Material materials with Biegemodul of 1.93 GPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 210 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 210 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 41.4 MPa Show Supplier Material materials with Zugfestigkeit of 41.4 MPa | ASTM D638 |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | UL 94 V0 (1.5mm) |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.5 - 0.7 % Show Supplier Material materials with Schrumpfung of 0.5 - 0.7 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Additives | Flame Retardant |