Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.55 g/cm³ Show Supplier Material materials with Dichte of 1.55 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 75.8 MPa Show Supplier Material materials with Biegefestigkeit of 75.8 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 1.79 GPa Show Supplier Material materials with Biegemodul of 1.79 GPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 530 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 530 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 66.2 MPa Show Supplier Material materials with Zugfestigkeit of 66.2 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 171 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 171 °C | ASTM D648 |
Technological properties
Property | ||
---|---|---|
Fillers | 40% Glass Fiber |