Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.63 g/cm³ Show Supplier Material materials with Dichte of 1.63 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 152 MPa Show Supplier Material materials with Biegefestigkeit of 152 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 8.27 GPa Show Supplier Material materials with Biegemodul of 8.27 GPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 53 J/m | ASTM D256 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 165 °C Show Supplier Material materials with Schmelzpunkt of 165 °C | ASTM D2117 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | ASTM D147 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |