Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.7 g/cm³ Show Supplier Material materials with Dichte of 1.7 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 159 MPa Show Supplier Material materials with Biegefestigkeit of 159 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 10.3 GPa Show Supplier Material materials with Biegemodul of 10.3 GPa | ASTM D790 |
Dehnung | 23.0 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 75 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 75 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 117 MPa Show Supplier Material materials with Zugfestigkeit of 117 MPa | ASTM D638 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.8E-4 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.8E-4 1/K | |
Wärmeformbeständigkeitstemperatur | 166 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 166 °C | ASTM D648 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | ASTM D147 |
Technological properties
Property | ||
---|---|---|
Fillers | 40% Glass Fiber |