Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.24 g/cm³ Show Supplier Material materials with Dichte of 1.24 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 5.63 GPa Show Supplier Material materials with Biegemodul of 5.63 GPa | ASTM D790 |
Härte, Shore D | 23.0 °C | 82 [-] Show Supplier Material materials with Härte, Shore D of 82 [-] | ASTM D785 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 64 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 64 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 78 MPa Show Supplier Material materials with Zugfestigkeit of 78 MPa | ASTM D638 |
Thermisch
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |