Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.18 g/cm³ Show Supplier Material materials with Dichte of 1.18 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 117 MPa Show Supplier Material materials with Biegefestigkeit of 117 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 7.58 GPa Show Supplier Material materials with Biegemodul of 7.58 GPa | ASTM D790 |
Dehnung | 23.0 °C | 1 % Show Supplier Material materials with Dehnung of 1 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 53 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 82.7 MPa Show Supplier Material materials with Zugfestigkeit of 82.7 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Wärmeformbeständigkeitstemperatur | 110 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 110 °C | ASTM D648 | |
Entflammbarkeit | UL 94 HB (1.6mm) |
Technological properties
Property | ||
---|---|---|
Fillers | 10% Carbon Fiber |